Help: the area around the weld turns black, with a ring of burn marks too. Is the gear too high, or was the nickel strip not pressed flat? 0.15 nickel-plated on the H1, I'm using gear 45.
It tears off when I give it a pull, so I don't feel good about putting it in a pack. Could any old hands point me in the right direction? Thanks!