57 settings stated on camera by creators, extracted from 137 videos; each row links to the project and the moment in the original clip.

CellMaterialWelderSettingSource
—Nickel strip (handles 0.4, per the seller); stainless utility-knife blade (test)UF20BGear 31 (rapid-fire); 99 (welded through a blade)Idle Honglin · Ep. 2 | Spot welde… · 01:07
—Nickel strip (included)UF20BGear Default 05, max 100 · Pulse width 20 msElectro Wu · Episode 732 · 01:37
—Copper strip (+ 0.12 nickel-plated steel strip base layer as control)UF20BGear 60CrazyFun · Welder at gear 60,… · 00:39
—0.15 nickel strip; can take 0.1–0.15 copper on topUF20B (P60F also on camera)Gear 30 (both welders compared); 40 (harsher)CrazyFun · Ep. 178 | The weld… · 00:27
—Stacked combinations: 0.15 nickel-plated + 0.1 copper + 0.15 nickel-plated; 0.1 nickel-plated + 0.15 copper + 0.1 nickel-plated; 0.15 nickel + 0.15 copper (thinner top layer)UF20B (upgraded to the No. 6 welding pen)Gear 20CrazyFun · Episode 183 | When… · 00:28

These are creators’ own settings as stated in their videos, not official AWithZ values; welder condition, tip wear and strip batch all matter — always test on scrap first.