Poll: Which cell do you weld most often these days?
The next Parameters table will be prioritized by vote count. After voting, tell us in the comments which combo you'd most like to see (material × thickness).
Parameters table update: new lab-tested entries for 0.1 / 0.15 copper
In the lab we welded 30 spots each on the UF20B, UK1 and P60F and took the median of the pull tests. Copper needs flux — without it the welds basically won't hold. This got asked in the comments so many times that we just wrote it into the table.
The table is on the "Parameters" page, filterable by cell × material × thickness.
Ran into a problem? Have an idea for improvement? Tell us. We read every piece of feedback carefully. Valid feedback earns points, redeemable for accessories / coupons.
Thanks for your feedback!
We'll review it within 1–5 business days. If you left an email, valid feedback earns points redeemable for accessories / coupons. If we need to follow up, we'll contact you at the email you left.
WeldWorld is an open platform for user sharing; content does not represent official advice.
Improper battery handling can cause fire, explosion, chemical burns and serious injury. Read the full AWithZ Safety & Usage Guidelines before any lithium battery assembly, spot welding or testing, and before using the community.
Community content is personal experience, not verified by AWithZ; where it conflicts with official documents, the official documents prevail.
Never apply someone else's settings directly; always start at a low level and test on scrap.
Before copying any procedure, go through the self-check list in Part 3 of the guidelines.