![【铝转镍】难题终结者![铝转镍焊接]难题终结者!AWithZ阿威兹P30C点焊机,轻松搞定高难度](/assets/community/works/d152/cover.jpg?v=647c4101)




First make sure the pins are pressed firmly and the surface is clean; start low and step up — 0.1–0.15mm Ni-plated steel usually needs only a low-to-mid level. Look up settings by cell model × material in the WeldWorld parameter lookup.
官方实验室最大值:镀镍钢带 0.8mm,纯镍带 0.4mm,紫铜带 0.2mm,不锈钢带 0.8mm。不同材料批次与环境有差异,先在废料上试焊。
Pins are consumables — dress or replace them when welds enlarge, spark often or blacken noticeably; see the manual's pin-change section and the Academy videos for steps.
Supercapacitor models need no charge maintenance — store them dry at room temperature; on next use, plug in for about 10 seconds to recharge.