First make sure the pins are pressed firmly and the surface is clean; start low and step up — 0.1–0.15mm Ni-plated steel usually needs only a low-to-mid level. Look up settings by cell model × material in the WeldWorld parameter lookup.
官方实验室最大值:镀镍钢带 0.25mm,纯镍带 0.15mm,不锈钢带 0.25mm,铁片 0.25mm。不同材料批次与环境有差异,先在废料上试焊。
Pins are consumables — dress or replace them when welds enlarge, spark often or blacken noticeably; see the manual's pin-change section and the Academy videos for steps.
锂电机型建议每 3 个月补电一次至 50–80%,避免高温与满电长期存放。