H1 FAQ
First make sure the pins are pressed firmly and the surface is clean; start low and step up — 0.1–0.15mm Ni-plated steel usually needs only a low-to-mid level. Look up settings by cell model × material in the WeldWorld parameter lookup.
Official lab maximums: Nickel-plated steel strip 0.25 mm, Pure nickel strip 0.15 mm, Copper strip 0.1 mm, Stainless strip 0.25 mm, Iron sheet 0.25 mm. Results vary with material batch and conditions — test on scrap first.
Pins are consumables — dress or replace them when welds enlarge, spark often or blacken noticeably; see the manual's pin-change section and the Academy videos for steps.
For lithium models, top up to 50–80% every three months; avoid heat and long-term storage at full charge.
Host warranty of 1–2 years by model (2 years for UF20B/UK3/HF7, 1 year for UK1/UKF10; accessories such as welding pens excluded); 7-day no-reason returns; invoices available for genuine flagship purchases
Share your experience
Tell us about issues with your H1, accessories you want, or feature ideas. Approved feedback earns an accessory coupon.